Pipe Dimension According to ANSI B 36.19
| Nominal Bore |
Outside Diameter |
Schedule 5S |
Schedule 10S |
Schedule 40S |
Schedule 80S |
Schedule 160S |
Schedule XXS |
| mm |
INCH |
mm |
Wt
mm |
Weight
(Kg/mt) |
Wt
mm |
Weight
(Kg/mt) |
Wt
mm |
Weight
(Kg/mt) |
Wt
mm |
Weight
(Kg/mt) |
Wt
mm |
Weight
(Kg/mt) |
Wt
mm |
Weight
(Kg/mt) |
| 3 |
1/8 |
10.3 |
1.24 |
0.276 |
1.24 |
0.28 |
1.73 |
0.37 |
2.41 |
0.47 |
- |
- |
- |
- |
| 6 |
1/4 |
13.7 |
1.24 |
0.390 |
1.65 |
0.49 |
2.24 |
0.631 |
3.02 |
0.80 |
- |
- |
- |
- |
| 10 |
3/8 |
17.1 |
1.24 |
0.490 |
1.65 |
0.63 |
2.31 |
0.845 |
3.20 |
1.10 |
- |
- |
- |
- |
| 15 |
1/2 |
21.3 |
1.65 |
0.800 |
2.11 |
1.00 |
2.77 |
1.27 |
3.75 |
1.62 |
4.75 |
1.94 |
7.47 |
2.55 |
| 20 |
3/4 |
26.7 |
1.65 |
1.03 |
2.11 |
1.28 |
2.87 |
1.68 |
3.91 |
2.20 |
5.54 |
2.69 |
7.82 |
3.63 |
| 25 |
1 |
33.4 |
1.65 |
1.30 |
2.77 |
2.09 |
3.38 |
2.50 |
4.55 |
3.24 |
6.35 |
4.24 |
9.09 |
5.45 |
| 32 |
1.1/4 |
42.2 |
1.65 |
1.65 |
2.77 |
2.70 |
3.56 |
3.38 |
4.85 |
4.47 |
6.35 |
5.61 |
9.70 |
7.77 |
| 40 |
1.1/2 |
48.3 |
1.65 |
1.91 |
2.77 |
3.11 |
3.68 |
4.05 |
5.08 |
5.41 |
7.14 |
7.25 |
10.16 |
9.54 |
| 50 |
2 |
60.3 |
1.65 |
2.40 |
2.77 |
3.93 |
3.91 |
5.44 |
5.54 |
7.48 |
8.74 |
11.1 |
11.07 |
13.44 |
| 65 |
2.1/2 |
73.0 |
2.11 |
3.69 |
3.05 |
5.26 |
5.16 |
8.63 |
7.01 |
11.4 |
9.53 |
14.9 |
14.2 |
20.39 |
| 80 |
3 |
88.9 |
2.11 |
4.51 |
3.05 |
6.45 |
5.49 |
11.30 |
7.62 |
15.2 |
11.1 |
21.3 |
15.24 |
27.65 |
| 100 |
4 |
114.3 |
2.11 |
5.84 |
3.05 |
8.36 |
6.02 |
16.07 |
8.56 |
22.3 |
13.49 |
33.54 |
17.12 |
41.03 |
| 125 |
5 |
141.3 |
2.77 |
9.47 |
3.40 |
11.57 |
6.55 |
21.8 |
9.53 |
31.97 |
15.88 |
49.11 |
19.05 |
57.43 |
| 150 |
6 |
168.3 |
2.77 |
11.32 |
3.40 |
13.84 |
7.11 |
28.3 |
10.97 |
42.7 |
18.2 |
67.56 |
21.95 |
79.22 |
| 200 |
8 |
219.1 |
2.77 |
14.79 |
3.76 |
19.96 |
8.18 |
42.6 |
12.7 |
64.6 |
23.0 |
111.2 |
22.23 |
107.8 |
| 250 |
10 |
273.1 |
3.40 |
22.63 |
4.19 |
27.78 |
9.27 |
60.5 |
12.7 |
96.0 |
28.6 |
172.4 |
25.40 |
155.15 |
| 300 |
12 |
323.9 |
3.96 |
31.25 |
4.57 |
36.00 |
9.52 |
73.88 |
12.7 |
132.0 |
33.32 |
238.76 |
25.40 |
186.97 |
| 350 |
14 |
355.6 |
3.96 |
34.36 |
4.78 |
41.3 |
11.13 |
94.59 |
19.05 |
158.08 |
35.71 |
281.70 |
- |
- |
| 400 |
16 |
406.4 |
4.19 |
41.56 |
4.78 |
47.29 |
12.7 |
123.30 |
21.41 |
203.33 |
40.46 |
365.11 |
- |
- |
| 450 |
18 |
457.2 |
4.19 |
46.80 |
4.78 |
53.42 |
14.27 |
155.80 |
23.8 |
254.36 |
45.71 |
466.40 |
- |
- |
| 500 |
20 |
508.0 |
4.78 |
59.25 |
5.54 |
68.71 |
15.09 |
183.42 |
26.19 |
311.2 |
49.99 |
564.68 |
- |
- |
| 600 |
24 |
609.6 |
5.54 |
82.47 |
6.35 |
94.45 |
17.48 |
255.41 |
30.96 |
442.08 |
59.54 |
808.22 |
- |
- |
| 650 |
26 |
660.4 |
|
|
7.92 |
129.40 |
9.53 |
155.32 |
12.70 |
205.97 |
- |
- |
- |
- |
| 700 |
28 |
711.2 |
|
|
7.92 |
139.47 |
9.53 |
167.44 |
12.70 |
222.13 |
- |
- |
- |
- |
| 750 |
30 |
762.0 |
6.35 |
120.15 |
7.92 |
149.55 |
9.53 |
179.56 |
12.70 |
238.28 |
- |
- |
- |
- |
| 800 |
32 |
812.8 |
- |
- |
7.92 |
159.62 |
9.53 |
191.69 |
12.70 |
254.44 |
- |
- |
- |
- |
| 850 |
34 |
863.6 |
- |
- |
7.92 |
169.64 |
9.53 |
203.74 |
12.70 |
270.50 |
- |
- |
- |
- |
| 900 |
36 |
914.4 |
- |
- |
7.92 |
179.77 |
9.53 |
215.93 |
12.70 |
286.75 |
- |
- |
- |
- |