Alloy 20 round bars are widely recognized for their exceptional resistance to corrosion, particularly in aggressive environments where other materials may fail. Alloy 20, also known as Carpenter 20 or Incoloy 20, is a nickel-chromium-molybdenum alloy that is specially designed to withstand sulfuric acid and other corrosive substances. It is highly resistant to pitting, crevice corrosion, and stress corrosion cracking, making it ideal for applications in industries such as chemical processing, pharmaceuticals, food production, and marine engineering.
Due to its wide range of beneficial properties, Alloy 20 round bars are in high demand across the globe. Importers, suppliers, stockists, and exporters play a vital role in ensuring the availability of this high-performance alloy for industries worldwide. These professionals source Alloy 20 round bars from reliable manufacturers and distribute them to customers based on specific requirements. Whether it's for large-scale industrial projects or smaller-scale applications, Alloy 20 round bars are available in various sizes and specifications to meet the needs of different industries.
The versatility of Alloy 20 round bars also lies in their ability to be easily fabricated into various shapes and sizes, allowing manufacturers to create custom solutions for specific needs. Its excellent machinability and weldability further enhance its attractiveness to industries that require precise components for complex designs. Additionally, Alloy 20’s resistance to high temperatures and its non-magnetic properties make it a preferred material in a wide range of specialized applications, from heat exchangers to valves and pumps.
Importers and suppliers typically stock a diverse range of Alloy 20 round bars, ensuring customers have access to the specific dimensions and grades they require. Stockists are particularly beneficial for customers who need immediate availability and quick turnaround times. Exporters, on the other hand, facilitate the global movement of Alloy 20 round bars, connecting manufacturers and industries from different parts of the world.
Alloy 20 round bars offer a unique combination of corrosion resistance, strength, and durability that make them a top choice for industries dealing with harsh environments. As importers, suppliers, stockists, and exporters continue to meet the global demand for this alloy, its applications are only expected to grow. Whether you're working on a large-scale project or looking for smaller quantities, Alloy 20 round bars are an indispensable material for ensuring the reliability and safety of industrial processes across the world.
| UNS No | N08020 |
|---|---|
| Standard | ASTM B473, ASME SB473 |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm thickness |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Thickness | 1.6mm to 100mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Round Bar, Square Bar, Hex(A/F) Bar, Rectangle Bar, Billet, Ingot, Forging, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Alloy 20 | 2.4660 | N08020 | 32.0 - 38.0 | 19.0 - 21.0 | - | 2.0 - 3.0 | Bal | 3.0 - 4.0 | 1.00 Max | - | - | 0.07 Max | 0.035 Max | 1.0 Max | 2.00 Max | P - 0.045 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Alloy 20 | 655 | 240 | 35 | 8.1 |