Incoloy 800H is a high-performance alloy known for its excellent resistance to oxidation, carburization, and high-temperature environments. This alloy is primarily composed of nickel, chromium, and iron, offering superior strength, stability, and corrosion resistance. Incoloy 800H wires are widely used in industries that demand materials that can withstand extreme temperatures and aggressive chemical conditions, such as in the power generation, petrochemical, and chemical processing sectors.
Incoloy 800H wires are specifically designed to perform in high-temperature environments, making them ideal for use in heat exchangers, furnace components, and reactor cores. The material exhibits outstanding resistance to oxidation and carburization at elevated temperatures, which is a common challenge for metals exposed to high heat. These properties ensure the long-term durability and reliability of Incoloy 800H wires, even in the harshest environments.
One of the key reasons for the widespread use of Incoloy 800H wires is their ability to maintain their strength and resistance to creep (the tendency of materials to deform permanently under stress over time) at elevated temperatures. This makes them an essential component in the manufacture of industrial equipment used in high-temperature processes.
Incoloy 800H wires are used in a variety of industrial applications due to their ability to withstand extreme temperatures and resist corrosion. These wires are commonly used in power plants, furnace construction, and in the production of heat exchangers. Additionally, they are used in nuclear reactors, petrochemical plants, and other industries where high heat resistance is critical. The versatility of Incoloy 800H wires makes them an essential material in industries that require reliable and long-lasting performance in harsh conditions.
Working with trusted suppliers and stockists ensures that businesses receive high-quality Incoloy 800H wires at competitive prices. These professionals are well-versed in the specifications and applications of Incoloy 800H, allowing them to provide expert advice and assistance in selecting the right wire for a specific application.
| UNS No | N08810 |
|---|---|
| Standard | Incoloy 800H Wires |
| Diameter | 0.1mm to 100mm |
| Length | 100mm to 6000mm, Custom Cut Length |
| Form | Filler Wire, Coil Wire, Wire, etc. |
| Grade | C | Mn | Si | Al | S | Cr | Cu | Ni | Fe | Ti |
|---|---|---|---|---|---|---|---|---|---|---|
| Incoloy 800H | 0.05 max | 1.00 max | 0.05 max | 0.02 max | 0.03 max | 19.50-23.50 | 1.50-3.00 | 38.0-46.0 | 22.0 min | 0.06 – 1.20 |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|---|
| Incoloy 800H | 8.14 g/cm3 | 1400 °C (2550 °F) | Psi – 80,000 , MPa – 550 | Psi – 32,000 , MPa – 220 | 30 % |