Super Duplex S32760 Sheets, Plates, and Coils are premium-grade stainless steel products renowned for their exceptional strength, corrosion resistance, and durability. These materials are widely sought after in industries such as oil and gas, chemical processing, marine engineering, and construction, where high performance under challenging conditions is essential. With a perfect balance of austenitic and ferritic stainless steel properties, Super Duplex S32760 offers superior mechanical and corrosion resistance, making it a preferred choice for demanding applications.
As leading importers, suppliers, stockists, and exporters of Super Duplex S32760 Sheets, Plates, and Coils, companies strive to meet the diverse requirements of global markets. These products are known for their excellent resistance to pitting, crevice corrosion, and chloride-induced stress corrosion cracking, even in harsh environments such as offshore oil rigs or chemical plants. Their high chromium, molybdenum, and nitrogen content enhances their overall corrosion resistance, ensuring a long service life and reduced maintenance costs.
Super Duplex S32760 Sheets are often used in manufacturing storage tanks, heat exchangers, and pressure vessels. Their exceptional weldability and machinability make them easy to fabricate, meeting precise industrial specifications. Plates crafted from this material are highly versatile and come in various sizes and thicknesses to cater to the requirements of different sectors. They are ideal for structural and mechanical components that demand high strength and resistance to corrosive media.
The coils, on the other hand, are widely used in the production of pipelines, flanges, and fittings. Thanks to their high yield strength and excellent dimensional stability, they contribute to efficient and reliable performance in critical operations. These coils are also preferred for creating equipment and components for desalination plants, as they can withstand high saline conditions without degradation.
Super Duplex S32760 Sheets, Plates, and Coils stand out as indispensable materials for applications demanding high performance and durability. Their unique combination of properties ensures they can handle extreme environments while maintaining their structural integrity. With a network of reliable importers, suppliers, stockists, and exporters, industries worldwide can access these high-quality products to drive innovation and efficiency in their operations.
| UNS No. | S32760 |
|---|---|
| Standard | Super Duplex S32760 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
|---|---|---|---|---|---|---|---|
| Super Duplex S32760 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80000 , MPa – 550 | Psi – 35000 , MPa – 240 | 40 % |