Titanium Gr 2 Sheets, Plates & Coils

Titanium Gr 2 Sheets, Plates, and Coils are highly sought-after products in the manufacturing, aerospace, medical, and chemical industries due to their exceptional properties. Known for its high strength-to-weight ratio, corrosion resistance, and biocompatibility, Titanium Gr 2 (Grade 2) is the most widely used commercially pure titanium. As a result, it is an ideal material for applications where durability, reliability, and performance are crucial. Importers, suppliers, stockists, and exporters of Titanium Gr 2 Sheets, Plates, and Coils play an essential role in making these premium materials accessible to industries across the globe.

Titanium Gr 2, with a purity of 99.2%, offers excellent resistance to oxidation, pitting, and stress corrosion cracking. Its superior corrosion resistance makes it ideal for use in harsh environments such as seawater, chlorides, and acids, as well as in high-temperature applications. This makes it the material of choice for the chemical processing industry, marine engineering, heat exchangers, and even the medical field for implants and surgical devices.

When it comes to Titanium Gr 2 Sheets, Plates, and Coils, these products are available in various thicknesses, widths, and lengths to cater to the diverse needs of manufacturers. Titanium sheets are commonly used in applications like architectural cladding, aircraft structures, and chemical equipment, where both strength and lightweight properties are required. Plates, on the other hand, are used for heavier-duty applications such as pressure vessels, heat exchangers, and structural components.

Titanium Gr 2 Sheets, Plates, and Coils, sourcing from reputable importers, suppliers, stockists, and exporters is essential. Importers bring these high-demand materials into countries where they are not readily available, ensuring that industries have access to top-quality titanium products. Suppliers provide these materials in bulk to manufacturers, ensuring a steady and reliable supply.

Titanium Gr 2 products meet stringent quality standards, and are certified by international standards such as ASTM B265, AMS 4911, and others. Whether for use in the aerospace industry or in corrosive environments, companies need assurance that the titanium products they source will perform optimally and meet all technical specifications.

UNS No. R50400
Standard Titanium Gr 2 Sheets, Plates & Coils
Thickness 0.1mm thk to 100mm thk
Width 100mm to 2000mm
length 100mm to 6000mm, Custom Cut length
Forms Coils, shims, plates, sheets, strips, flats.
finish Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc.
Hardness Soft, Hard, Half Hard, Quarter hard, Spring hard etc.

Grade C N O H Ti Fe
Titanium Gr 2 0.10 max 0.03 max 0.25 max 0.015 max bal 0.30 max

Min.Tensile(KSI) Min.Yield(KSI) Hardness Tensile Modulus Poisson's Ratio
50 40 14.9 103 GPa 0.34 - 0.10

Application of Titanium Gr 2 Sheets, Plates & Coils

Power Plants Industry

Aerospace Industry

Refineries Industry

Oil & Gas Industry

Sugar Industry

Chemical Industry

Petrochemical Industry