Inconel 600 is a high-performance nickel-chromium alloy known for its excellent resistance to oxidation, corrosion, and high temperatures. Delta Superalloys stands out as a trusted supplier, stockist, importer, and exporter of premium-quality Inconel 600 fittings, flanges, and fasteners. These components are widely used in demanding industries such as aerospace, power generation, chemical processing, and marine engineering, where durability and reliability are paramount.
Inconel 600 fittings are designed to deliver superior performance in environments prone to extreme temperature fluctuations and corrosive agents. These fittings are ideal for applications in heat exchangers, nuclear reactors, and petrochemical plants. Delta Superalloys offers a wide range of fittings, including elbows, tees, reducers, and couplings, ensuring compatibility with diverse industrial systems. Their precision-engineered fittings are manufactured to meet global quality standards, making them a preferred choice for importers and exporters alike.
Delta Superalloys provides an extensive selection, including slip-on, weld neck, socket weld, and blind flanges. These flanges are designed to provide secure and leak-proof connections in high-pressure and high-temperature environments. The excellent mechanical properties and oxidation resistance of Inconel 600 ensure that these flanges maintain their integrity even under challenging conditions, making them a valuable asset for stockists and suppliers serving global markets.
Inconel 600 fasteners, such as bolts, nuts, washers, and screws, play a critical role in maintaining structural stability in harsh environments. Delta Superalloys' fasteners are crafted to endure exposure to extreme temperatures and corrosive chemicals, ensuring long-term performance and safety. These fasteners are extensively used in oil and gas exploration, chemical processing plants, and thermal processing equipment, highlighting their versatility and reliability.
In addition to high-quality products, Delta Superalloys emphasizes customer satisfaction through competitive pricing, timely deliveries, and exceptional service. Their expertise in the field ensures that every product meets stringent quality standards, whether supplied to stockists, direct end-users, or other suppliers. As a reliable partner, Delta Superalloys has established itself as a leader in the export and supply of Inconel 600 components worldwide.
| UNS No. | N06600 |
|---|---|
| Standards | Inconel 600 Fittings, Flanges & Fastners |
| Fitting Size | 1/2"NB to 36"NB |
| Fitting Thickness | SCH55, SCH10S, SCH40S, SCH50S, SCH100S, SCH120S, SCH5, SCH10, SCH40, SCH80, SCH100, SCH120, SCH160, SCH140, SCH160, SCH XXS |
| Type | Seamless/Welded/Fabricated |
| Flange Size | 1/2"NB to 36"NB |
| Flange Class | 150#, 300#, 900#, 600#, 1500# |
| Flange Type | Weld neck, Slip on, Blind, Socket weld, (WNRF, BLRF, SORF, SOFF) |
| Fasteners Size | M3 to M80, 1/8" to 70", Custom size |
| Fasteners Length | 3mm to 300mm |
| Bolt Type | Hex head bolts, Square Bolts, T Bolts, U8 Bolts, Dome Bolt, etc |
| Screw Type | Hex head Screw, Socket head Screw, Socket set Screw, etc |
| Studs Types | Double Ended Studs, Threaded Rod, Tie Bars, etc |
| Washer Types | Plain Washers, Lock Washers, Star Washer, etc |
| Nut Types | Hex Nut, Lock Nut, Dome Nut, Square Nut, Coupling Nut, etc |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 600 | 2.4816 | N06600 | 72.00 | 14.0 - 17.0 | - | - | 6.0 - 10.0 | 0.50 Max | - | 0.30 Max | 0.3 Max | 0.05 - 0.15 | 0.015 Max | 0.50 Max | 1.00 Max | B - 0.006 Max / P - 0.015 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel 600 | 620 | 275 | 30 | 8.47 |