Delta Superalloys offers a wide range of Inconel 600 Wire, which are normally preferred for handling concentrated and high temperature caustic. Its high nickel content, a minimum of Ni 72 %, combined with its chromium content, provides users of Inconel 600 Wire a number of benefits.
In strong oxidizing solutions like hot, concentrated nitric acid, Inconel 600 Coil Wire has poor resistance. The high chromium content of Inconel 600 Wire raises its oxidation resistance considerably above that of pure nickel, while its high nickel content provides good corrosion resistance under reducing conditions.
Inconel 600 Wire can both hot formed and cold form using typical processes, and is also often used in vegetable and fatty acid vessels. Inconel 600 Wire is also used for furnace components, in food and chemical processing, nuclear engineering, and sparking electrodes. Chromium content in Alloy 600 Coiled Wire confers resistance to sulfur compounds and also provides resistance to oxidizing conditions at high temperatures or in corrosive solutions.
The high nickel content in Alloy 600 Coil Wire enables it to retain considerable resistance under reducing conditions. Alloy 600 Wire is a nickel – chromium alloy with good oxidation resistance at high temperatures and resistance to chloride – ion stress – corrosion cracking, corrosion by high – purity water, and caustic corrosion. Alloy 600 Wire has exceptional Temperature Resistance and Corrosion Resistance as its excellent properties.
| UNS No | N06600 |
|---|---|
| Standard | Inconel 600 Wires |
| Diameter | 0.1mm to 100mm |
| Length | 100mm to 6000mm, Custom Cut Length |
| Form | Filler Wire, Coil Wire, Wire, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 600 | 2.4816 | N06600 | 72.00 | 14.0 - 17.0 | - | - | 6.0 - 10.0 | 0.50 Max | - | 0.30 Max | 0.3 Max | 0.05 - 0.15 | 0.015 Max | 0.50 Max | 1.00 Max | B - 0.006 Max / P - 0.015 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel 600 | 620 | 275 | 30 | 8.47 |