Hastelloy 600 round bars are a premium-grade material widely used in industries requiring exceptional heat and corrosion resistance. Manufactured by Delta Superalloys, these bars are crafted to meet the demanding needs of various applications, particularly in environments with extreme temperatures and oxidative stress. Known for their superior performance, these round bars are an ideal choice for applications in aerospace, power generation, and chemical processing industries.
Inconel 600 belongs to a family of austenitic superalloys. The Inconel 600 Round Bar is made with a chemical composition comprising of carbon, nickel, manganese, silicon, ferrous, sulfur, chromium, and copper. These bars possess superior strength and are resistant to corrosion and erosion in stress-induced environments.
The Alloy 600 Rod doesn’t deform or dissociate easily under extreme pressures and elevated temperatures. These rods are available in standard sizes between 5mm to 500mm which can be customized on request. The UNS N06600 Hex bar possesses good mechanical properties and enhanced hardness.
These bars possess a minimum tensile strength of 655Mpa and a minimum yield strength of 310Mpa. They can be elongated by 40% and still exhibit excellent machinability. We are the top Inconel 600 Round Bar suppliers in the country. Our goal is to supply high-quality products to all our clients at reasonable rates.
The Nickel Alloy 600 Square Bar is widely used in industrial set-ups. These bars are in demand as they can be employed in general repairs, manufacturing, and general assembly. They are available in sizes between 4mm to 100mm. The DIN 2.4816 flat Bar is produced in the shape of long metal bars. These bars act as supporting materials and are used in different structural and architectural applications. This Inconel 600 Flat Bar is very reliable in stress-induced environments. These bars are available in standard thicknesses up to 100mm and widths between 10mm to 500mm.
| UNS No | N06600 |
|---|---|
| Standard | Inconel 600 Round Bars |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm thickness |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Thickness | 1.6mm to 100mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Round Bar, Square Bar, Hex(A/F) Bar, Rectangle Bar, Billet, Ingot, Forging, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 600 | 2.4816 | N06600 | 72.00 | 14.0 - 17.0 | - | - | 6.0 - 10.0 | 0.50 Max | - | 0.30 Max | 0.3 Max | 0.05 - 0.15 | 0.015 Max | 0.50 Max | 1.00 Max | B - 0.006 Max / P - 0.015 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel 600 | 620 | 275 | 30 | 8.47 |