Delta Superalloys is a trusted name in the industry, known for its high-quality Inconel X-750 fittings, flanges, and fasteners. As leading importers, suppliers, stockists, and exporters, we specialize in delivering premium products that meet the diverse requirements of various industrial sectors. Our extensive inventory, global presence, and commitment to excellence make us a reliable partner for your material needs.
Inconel X-750 is a nickel-chromium alloy designed for high-performance applications requiring superior strength, corrosion resistance, and durability under extreme conditions. This alloy is precipitation-hardenable, which means it maintains its mechanical integrity in high-temperature environments. Commonly used in aerospace, power generation, and chemical processing industries, Inconel X-750 is a preferred choice for components that must endure stress, heat, and corrosive environments over extended periods.
Our range of Inconel X-750 fittings includes elbows, tees, reducers, and caps, all engineered to provide exceptional reliability in demanding environments. These fittings are widely used in applications such as piping systems for high-temperature and high-pressure conditions. Delta Superalloys ensures that each fitting meets international standards like ASTM and ASME, delivering products that combine precision with performance.
As one of the most reputable importers, suppliers, stockists, and exporters of Inconel X-750 fittings, flanges, and fasteners, Delta Superalloys stands out for its customer-centric approach and unwavering commitment to quality. We maintain a comprehensive inventory to ensure quick delivery and support clients across industries with tailored solutions. Our products are subjected to rigorous quality checks and are certified to meet the highest international standards.
| UNS No. | N07750 |
|---|---|
| Standards | Inconel X-750 Fittings, Flanges & Fastners |
| Fitting Size | 1/2"NB to 36"NB |
| Fitting Thickness | SCH55, SCH10S, SCH40S, SCH50S, SCH100S, SCH120S, SCH5, SCH10, SCH40, SCH80, SCH100, SCH120, SCH160, SCH140, SCH160, SCH XXS |
| Type | Seamless/Welded/Fabricated |
| Flange Size | 1/2"NB to 36"NB |
| Flange Class | 150#, 300#, 900#, 600#, 1500# |
| Flange Type | Weld neck, Slip on, Blind, Socket weld, (WNRF, BLRF, SORF, SOFF) |
| Fasteners Size | M3 to M80, 1/8" to 70", Custom size |
| Fasteners Length | 3mm to 300mm |
| Bolt Type | Hex head bolts, Square Bolts, T Bolts, U8 Bolts, Dome Bolt, etc |
| Screw Type | Hex head Screw, Socket head Screw, Socket set Screw, etc |
| Studs Types | Double Ended Studs, Threaded Rod, Tie Bars, etc |
| Washer Types | Plain Washers, Lock Washers, Star Washer, etc |
| Nut Types | Hex Nut, Lock Nut, Dome Nut, Square Nut, Coupling Nut, etc |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel X-750 | 2.4669 | N07750 | 70.00 Min | 14.0 - 17.0 | 1.00 Max | - | 5.0 - 9.0 | 0.50 Max | 0.70 - 1.20 | 0.40 - 1.0 | 2.25 - 2.75 | 0.08 Max | 0.01 Max | 0.50 Max | 1.00 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel x-750 | 1200 | 820 | 30 | 8.28 |