Inconel X-750 is a nickel-chromium alloy renowned for its excellent resistance to high temperatures, oxidation, and corrosion. This versatile material is used extensively in applications requiring superior strength and stability under extreme conditions. Delta Superalloys is a leading name in the production and distribution of Inconel X-750 forged products, offering high-quality solutions to industries worldwide.
Forged products made from Inconel X-750 are favored for their exceptional mechanical properties and remarkable resistance to stress cracking, creep, and thermal fatigue. These characteristics make them a preferred choice for aerospace, gas turbines, nuclear reactors, and petrochemical industries. At Delta Superalloys, the forging process is meticulously carried out to ensure the products meet stringent international standards, catering to the specific demands of various applications.
As prominent importers, suppliers, stockists, and exporters of Inconel X-750 forged products, Delta Superalloys ensures a steady supply chain for businesses across the globe. Their extensive inventory includes a wide range of forged components such as rings, discs, shafts, and flanges, all available in custom dimensions and configurations. By maintaining a robust stock, the company reduces lead times, providing customers with prompt delivery without compromising on quality.
The forging process enhances the strength and durability of Inconel X-750 products, ensuring superior performance in demanding environments. This alloy is highly resistant to oxidation and retains its strength even at elevated temperatures, making it indispensable in the manufacturing of jet engines, spacecraft, and power generation equipment. Delta Superalloys employs advanced forging techniques and precision engineering to produce components that excel in reliability and longevity.
| UNS No | N07750 |
|---|---|
| Standard | Inconel X-750 Forged Products |
| Circle | 5mm dia to 2000mm dia |
| Thickness | 6mm thk to 500mm thk |
| Flat Bar Blocks | 5mm thk to 500mm thk |
| Rings | 50mm dia to 1000mm dia |
| Rounds, shafts | 6mm dia to 500mm dia |
| Hex Bar | 6mm dia to 500mm dia |
| Cylinder and sleeves | 6mm dia to 500mm dia |
| Finish | Black or Bright |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel X-750 | 2.4669 | N07750 | 70.00 Min | 14.0 - 17.0 | 1.00 Max | - | 5.0 - 9.0 | 0.50 Max | 0.70 - 1.20 | 0.40 - 1.0 | 2.25 - 2.75 | 0.08 Max | 0.01 Max | 0.50 Max | 1.00 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel x-750 | 1200 | 820 | 30 | 8.28 |