Hastelloy X Pipe fittings are high-conducting iron nickel-chromium-molybdenum alloy that sustains corrosion. They are highly durable. Hastelloy X Pipe Fittings are best suited for oxidation. These pipe fittings can perform well at high temperatures. In the case of reducing atmospheres, they are immune to cracking. They also resist carburization. These Pipe fittings exhibit non-magnetism. Their high melting point is the reason for their great strength at varying temperatures.
Hastelloy X flanges are high-performance chromium-nickel iron molybdenum super alloy flanges that possess superior corrosion resistance consistency and durability. These alloy of flanges primarily noted for good oxidation and heat resistance. Therefore these flanges exhibit superior resistance to carburization and chloride stress corrosion cracking in reducing atmospheres. Thus these alloys of flanges are basically non-magnetic but feature superior higher strength at a temperature range of 1500 degree F. whereas show good oxidation resistance up to 2200 degree F.
High-performance Hastelloy X Flanges are chromium-nickel iron-molybdenum super alloy flanges with superior corrosion resistance, stability, and durability. These alloy flanges are primarily recognized for their strong oxidation and heat resistance.
Due to their superior resistance to carburization and chloride stress corrosion cracking in reducing atmospheres, these flanges are a good choice to be used in these environments. Therefore, these flange alloys are essentially non-magnetic but exhibit superior greater strength at temperatures up to 1500 °, while exhibiting good oxidation resistance up to 2200 ℉.
In forming and welding, this alloy works well. Some characteristics of the Hastelloy X Flanges are resistance to a wide range of corrosive mediums, non-magnetic, and excellent mechanical properties. These flanges have outstanding hardness and toughness. It also possesses thermal conductivity and electrical resistivity.
| UNS No. | N06002 |
|---|---|
| Standards | Hastelloy X Fittings, Flanges & Fastners |
| Fitting Size | 1/2"NB to 36"NB |
| Fitting Thickness | SCH55, SCH10S, SCH40S, SCH50S, SCH100S, SCH120S, SCH5, SCH10, SCH40, SCH80, SCH100, SCH120, SCH160, SCH140, SCH160, SCH XXS |
| Type | Seamless/Welded/Fabricated |
| Flange Size | 1/2"NB to 36"NB |
| Flange Class | 150#, 300#, 900#, 600#, 1500# |
| Flange Type | Weld neck, Slip on, Blind, Socket weld, (WNRF, BLRF, SORF, SOFF) |
| Fasteners Size | M3 to M80, 1/8" to 70", Custom size |
| Fasteners Length | 3mm to 300mm |
| Bolt Type | Hex head bolts, Square Bolts, T Bolts, U8 Bolts, Dome Bolt, etc |
| Screw Type | Hex head Screw, Socket head Screw, Socket set Screw, etc |
| Studs Types | Double Ended Studs, Threaded Rod, Tie Bars, etc |
| Washer Types | Plain Washers, Lock Washers, Star Washer, etc |
| Nut Types | Hex Nut, Lock Nut, Dome Nut, Square Nut, Coupling Nut, etc |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy X | 2.4665 | N06002 | Remainder | 20.5 - 23.0 | 0.50 - 2.5 | 8.0 - 10.0 | 17-20 | 0.50 Max | - | 0.50 Max | 0.15 Max | 0.05-0.15 | 0.03 Max | 1.00 Max | 1.00 Max | P-0.04 Max / W-0.2-1 / B-0.008 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy X | 755 | 385 | 49.50 | 8.22 |