Delta Superalloys offers Hastelloy Alloy X Sheets Plates and Coils in an extensive range, where our crew members make it a point to inspect these products on stern quality limits in order to be sure of their seamless toughness. However, procedures of Hastelloy X Plates are outstanding in terms of welding and forming. Hastelloy X Coils is an iron – molybdenum – nickel – chromium alloy that holds an excellent grouping of oxidation resistance, high temperature power and formability.
Hastelloy X Slatting Coils offers robust potency features at high temperatures up to 2200 degree F. An iron – molybdenum – nickel – chromium alloy, Hastelloy X Perforated Coils offers excellent casting characteristics and excellent creep-and-stress rupture attributes. Meanwhile, these Alloy X Plates are also being offered in customized sizes and shapes to our customers. Alloy X Coils also resists sulfuric, phosphoric, formic, acetic acids and other non – oxidizing media.
In addition to having exceptional corrosion resistance, Alloy X Slatting Coils can also be readily fabricated. Alloy X Perforated Coils exhibits superior welding conditions, providing excellent as – welded conditions for process applications in chemical – based industries such as food, beverage, personal care, and pharmaceutical.
The high chromium content in Hastelloy UNS N06002 Sheets provides good resistance to oxidizing media while the molybdenum and tungsten content give good resistance to reducing media. Alloy N06002 Plates is an ideal material for using in the diverse chemical processes in the as – welded situation.
| UNS No. | N06002 |
|---|---|
| Standard | Hastelloy X Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy X | 2.4665 | N06002 | Remainder | 20.5 - 23.0 | 0.50 - 2.5 | 8.0 - 10.0 | 17-20 | 0.50 Max | - | 0.50 Max | 0.15 Max | 0.05-0.15 | 0.03 Max | 1.00 Max | 1.00 Max | P-0.04 Max / W-0.2-1 / B-0.008 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy X | 755 | 385 | 49.50 | 8.22 |