We are providing Hastelloy X forged products in several sizes, types, shapes, grades and standards. We are importing these forged products in custom made specifications as per the demands. Hastelloy X has exceptional resistance to crevice corrosion and pitting. This alloy contains chromium, iron, molybdenum and tungsten. These elements provide excellent corrosion resistance in acidic and chloride environments.
Hastelloy X, a nickel-based superalloy, offers exceptional resistance to oxidation and corrosion, even at high temperatures. It is widely used in industries such as aerospace, chemical processing, and power generation. Its superior strength and excellent weldability make it ideal for critical applications like gas turbines, jet engine components, and industrial furnaces.
Delta Superalloys takes pride in providing Hastelloy X forged products in various forms, including forged rings, discs, shafts, and custom shapes tailored to specific project needs.One of the standout qualities of Delta Superalloys is their commitment to maintaining strict quality standards. As reputable suppliers of Hastelloy X forged products, they ensure that each piece undergoes rigorous testing and inspection to guarantee optimum performance.
Their products are manufactured using advanced forging techniques, ensuring a uniform grain structure and enhanced mechanical properties. This meticulous process enhances the material's resistance to high-temperature oxidation and thermal fatigue, which are crucial for applications in harsh environments.
| UNS No | N06002 |
|---|---|
| Standard | Hastelloy X Forged Products |
| Circle | 5mm dia to 2000mm dia |
| Thickness | 6mm thk to 500mm thk |
| Flat Bar Blocks | 5mm thk to 500mm thk |
| Rings | 50mm dia to 1000mm dia |
| Rounds, shafts | 6mm dia to 500mm dia |
| Hex Bar | 6mm dia to 500mm dia |
| Cylinder and sleeves | 6mm dia to 500mm dia |
| Finish | Black or Bright |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy X | 2.4665 | N06002 | Remainder | 20.5 - 23.0 | 0.50 - 2.5 | 8.0 - 10.0 | 17-20 | 0.50 Max | - | 0.50 Max | 0.15 Max | 0.05-0.15 | 0.03 Max | 1.00 Max | 1.00 Max | P-0.04 Max / W-0.2-1 / B-0.008 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy X | 755 | 385 | 49.50 | 8.22 |