The round bars are long and cylindrical metal bars that have many industrial and commercial applications. Inconel 625 alloy consists of nickel, chromium, and molybdenum in the composition, along with niobium. The molybdenum, along with niobium, helps the Inconel 625 Round Bar to have high strength without any strengthening heat-treatment process.
The Inconel 625 Round Bar offers extreme resistance to corrosion in various and extremely corrosive environments. Being one of the top Inconel round bar Suppliers, we can assure that the Inconel 625 material is high in durability and toughness. The Alloy 625 Rod is also known for its resistance to crevice corrosion and pitting. Apart from these, the Uns N06625 Hex Bar also has high fatigue strength and is resistant to stress corrosion cracking to chloride ions. The Inconel 625 Forged Bar is also resistant to caustics.
The Alloy 625 Rod doesn’t deform or dissociate easily under extreme pressures and elevated temperatures. These rods are available in standard sizes between 5mm to 500mm which can be customized on request. The UNS N06600 Hex bar possesses good mechanical properties and enhanced hardness.
The Alloy 625 cold drawn bar can serve in extreme environments depending on the amount of heat and pressure. It is one of the main reasons behind the popularity of these bars across industries. During the heat treatment, the 625 Inconel Alloy Hot rolled bar forms a thick and stable oxide layer around itself, which helps to protect the surface from different attacks.
We have clients demanding Inconel 625 Round Bar from different parts of the world; hence we take extra care of the packaging. We put each of the Inconel 625 Flat Bar in wooden pallets or boxes to not get damaged during transportation. No matter how big or small the consignment is, we will always take care of the Inconel 625 Hex Bar until it reaches your doorstep.
| UNS No | N06625 |
|---|---|
| Standard | Inconel 625 Round Bars |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm thickness |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Thickness | 1.6mm to 100mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Round Bar, Square Bar, Hex(A/F) Bar, Rectangle Bar, Billet, Ingot, Forging, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 625 | 2.4856 2.4831 | N06625 | 58.00 Min | 20.0 - 23.0 | 1.00 Max | 8.0 - 10.0 | 5.00 Max | - | 3.15 - 4.15 | 0.40 Max | 0.4 Max | 0.10 Max | 0.015 Max | 0.50 Max | 0.50 Max | P - 0.015 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel 625 | 827 | 414 | 40 | 8.44 |