Ganpat Industrial Corporation offers a wide range of Inconel 625 Wire , where pitting and crevice corrosion are prevented by molybdenum. These elements also contribute to these Inconel 625 Wires’ outstanding corrosion resistance. Our Inconel 625 Wire is resistant to seawater, in both flowing and stagnant conditions, and under fouling.
This Inconel 625 Coil Wire is resistant to pitting, impingement corrosion, crevice corrosion, inter – granular attack and is almost immune to chloride stress corrosion cracking.
Our Inconel 625 Electrode is often used in Bubble caps, Heat shields, Valves, Piping, Tubing, Distillation columns, Combustion and chimney liners. This Inconel 625 Wire is also used in Marine Industries, Chemical Processing, Aerospace Industries, Pollution Control, and Nuclear Reactors. Our Inconel 625 Wire has good resistance to oxidation and scaling at high temperatures.
This Alloy 625 Wire was designed as a solid solution strengthened material with no significant microstructure. High tensile, creep, and rupture strength; outstanding fatigue and thermal – fatigue strength; oxidation resistance; and excellent weldability and brazeability are the properties of our Alloy 625 Coil Wire that make it interesting to the aerospace field.
This Alloy 625 Wire has high creep – rupture strength, non – magnetic, and oxidation resistant to 1800 Degree F. Niobium stabilizes Alloy 625 Electrode against sensitization during welding. This Alloy 625 Wire has almost complete freedom from chloride induced stress corrosion cracking.
| UNS No | N06625 |
|---|---|
| Standard | Inconel 625 Wires |
| Diameter | 0.1mm to 100mm |
| Length | 100mm to 6000mm, Custom Cut Length |
| Form | Filler Wire, Coil Wire, Wire, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 625 | 2.4856 2.4831 | N06625 | 58.00 Min | 20.0 - 23.0 | 1.00 Max | 8.0 - 10.0 | 5.00 Max | - | 3.15 - 4.15 | 0.40 Max | 0.4 Max | 0.10 Max | 0.015 Max | 0.50 Max | 0.50 Max | P - 0.015 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel 625 | 827 | 414 | 40 | 8.44 |