As a well-known suppliers, we offer these Inconel 625 Sheets in a wide range to our clients. Inconel 625 Plates (UNS N06625) exhibits good restraint welding characteristics. During machining these Alloy 625 Sheets work harden rapidly, generate high heat during cutting, weld to the cutting tool surface and offer high resistance to metal removal because of their high shear strengths. Heavy restrained sections can be welded and the weld's mechanical properties follow the same trends as base metal properties.
These Alloy 625 Plates are used for several applications such as in Flare stacks, Seawater components, Chemical process equipment handling mixed acids both oxidizing and reducing, etc. Delta Superalloys also offers our clients a wide range of customized sizes and shapes of this product.
The thickness of the Inconel 625 sheet might vary based on the application and needs. Inconel 625 sheet is typically offered in thicknesses ranging from 0.016 inches to 0.187 inches (0.4 mm to 4.75 mm). While thicker sheets are frequently used in applications requiring high strength and resistance to extreme temperatures, such as those in the aerospace industry, thinner sheets are commonly used in applications requiring high-temperature corrosion resistance, such as those in the chemical processing industry.
A nickel-based alloy called Inconel 625 is renowned for its high strength, outstanding resistance to corrosion, and capacity to sustain extremely high temperatures. Due to these characteristics, Inconel 625 plates are advantageous and suitable for applications requiring high strength, corrosion resistance, and resistance to high temperatures. In the chemical processing and aerospace industries, Inconel 625 plates are usually used to construct machinery subject to corrosive chemicals and high temperatures.
The fabrication of the Inconel 625 sheet & plate is strictly conducted by using the high quality of alloy that is sourced from reputable market vendors. The alloy before used for the sheet and plates fabrication is very well tested to assure high quality of production. There at the well-equipped industry, the professional expert team is hired that are having all good skills and years of experience in fabrication of the product in a better way.
| UNS No. | N06625 |
|---|---|
| Standard | Inconel 625 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 625 | 2.4856 2.4831 | N06625 | 58.00 Min | 20.0 - 23.0 | 1.00 Max | 8.0 - 10.0 | 5.00 Max | - | 3.15 - 4.15 | 0.40 Max | 0.4 Max | 0.10 Max | 0.015 Max | 0.50 Max | 0.50 Max | P - 0.015 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Inconel 625 | 827 | 414 | 40 | 8.44 |