Monel 400, a nickel-copper alloy renowned for its excellent corrosion resistance and high strength, is a preferred material for various industrial applications. This alloy is particularly valued in industries like marine, chemical processing, and oil and gas, where exposure to harsh environments, including saltwater and acidic conditions, demands robust and durable materials. Monel 400 fittings, flanges, and fasteners are essential components that cater to these demanding sectors.
Monel 400 fittings are widely used for joining and routing pipes and tubing in systems exposed to aggressive media. These fittings include elbows, tees, reducers, and couplings, designed to provide secure connections and ensure leak-proof operations. Their exceptional resistance to stress-corrosion cracking, pitting, and oxidation makes them ideal for seawater applications, heat exchangers, and chemical handling systems. Leading suppliers and stockists of Monel 400 fittings maintain a vast inventory to meet the needs of industries worldwide, ensuring availability in various sizes, shapes, and pressure ratings.
Flanges are critical in connecting pipes, valves, and other equipment, enabling efficient assembly and disassembly for maintenance. Monel 400 flanges are prized for their ability to withstand extreme temperatures and corrosive environments. Available in types such as slip-on, weld neck, socket weld, and blind flanges, these components ensure reliable performance even under challenging operating conditions. Exporters and importers of Monel 400 flanges play a crucial role in distributing these products globally, catering to the growing demand for high-quality piping solutions.
Fasteners, including bolts, nuts, screws, and washers made from Monel 400, are indispensable in applications requiring superior mechanical properties and corrosion resistance. They are widely used in industries like offshore oil drilling, power plants, and aerospace, where material reliability is non-negotiable. Monel 400 fasteners retain their integrity under high pressures and in corrosive environments, making them a trusted choice among engineers and procurement specialists. Reputable stockists and exporters ensure that these fasteners meet international standards, guaranteeing quality and performance.
Monel 400’s versatility, coupled with its unparalleled resistance to corrosion and high mechanical strength, makes it a superior choice for critical applications. Businesses looking for reliable solutions in harsh environments benefit from partnering with trusted suppliers, stockists, and exporters specializing in Monel 400 products. This ensures access to top-quality components that meet stringent industry standards.
| UNS No. | N04400 |
|---|---|
| Standards | Monel 400 Fittings, Flanges & Fastners |
| Fitting Size | 1/2"NB to 36"NB |
| Fitting Thickness | SCH55, SCH10S, SCH40S, SCH50S, SCH100S, SCH120S, SCH5, SCH10, SCH40, SCH80, SCH100, SCH120, SCH160, SCH140, SCH160, SCH XXS |
| Type | Seamless/Welded/Fabricated |
| Flange Size | 1/2"NB to 36"NB |
| Flange Class | 150#, 300#, 900#, 600#, 1500# |
| Flange Type | Weld neck, Slip on, Blind, Socket weld, (WNRF, BLRF, SORF, SOFF) |
| Fasteners Size | M3 to M80, 1/8" to 70", Custom size |
| Fasteners Length | 3mm to 300mm |
| Bolt Type | Hex head bolts, Square Bolts, T Bolts, U8 Bolts, Dome Bolt, etc |
| Screw Type | Hex head Screw, Socket head Screw, Socket set Screw, etc |
| Studs Types | Double Ended Studs, Threaded Rod, Tie Bars, etc |
| Washer Types | Plain Washers, Lock Washers, Star Washer, etc |
| Nut Types | Hex Nut, Lock Nut, Dome Nut, Square Nut, Coupling Nut, etc |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Monel 400 | 2.4360 | N04400 | 63.00 Min | - | - | - | 2.5 Max | 28.0 - 34.0 | - | - | - | 0.30 Max | 0.024 Max | 0.50 Max | 2.0 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Monel 400 | 550 | 275 | 30 | 8.80 |