The Monel 400 Round Bars contain copper and nickel, having excellent strength and corrosion resistance properties. Monel 400 Round Bars offer incredible strength and flexibility in various temperatures. Its ideal general corrosion resistance property makes it extensively suitable for numerous industrial applications. Monel 400 provides resistance to pitting and crevice corrosion cracking, even under extreme conditions.
Monel 400 Round Bars are a highly sought-after product in industries that demand exceptional strength, corrosion resistance, and versatility. Fabricated from the Monel 400 alloy, these bars exhibit a remarkable combination of nickel and copper, ensuring excellent resistance to harsh environments, including seawater, acid, and alkaline conditions. Their durability and performance have made them a favorite choice among importers, suppliers, stockists, and exporters catering to the marine, chemical, and aerospace industries.
One of the standout properties of Monel 400 Round Bars is their resistance to stress corrosion cracking and pitting, even in the most demanding environments. This makes them ideal for applications such as pump shafts, propeller shafts, and seawater valves, where long-term reliability is essential. With the ability to withstand high temperatures and pressures, these bars are also used extensively in heat exchangers, boiler feedwater heaters, and nuclear plants.
Monel 400 Round Bars are also valued for their ease of fabrication and weldability, which allow manufacturers to customize them for specific applications. Their machinability ensures precision during production, making them suitable for complex and critical designs. This feature attracts industries looking for high-performance materials with minimal maintenance requirements, further driving their demand.
Monel 400 Round Bars are a versatile and durable solution for industries requiring superior material performance. Importers, suppliers, stockists, and exporters work collaboratively to meet the ever-growing demand for these bars, ensuring quality and reliability at every stage. Whether for marine, chemical, or industrial use, Monel 400 Round Bars stand out as a dependable and efficient choice.
| UNS No | N04400 |
|---|---|
| Standard | Monel 400 Round Bars |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm thickness |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Thickness | 1.6mm to 100mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Round Bar, Square Bar, Hex(A/F) Bar, Rectangle Bar, Billet, Ingot, Forging, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Monel 400 | 2.4360 | N04400 | 63.00 Min | - | - | - | 2.5 Max | 28.0 - 34.0 | - | - | - | 0.30 Max | 0.024 Max | 0.50 Max | 2.0 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Monel 400 | 550 | 275 | 30 | 8.80 |