Monel 400, a nickel-copper alloy renowned for its outstanding corrosion resistance and strength, is a top choice for various industrial applications. This versatile alloy contains approximately 67% nickel and 23% copper, making it ideal for environments where high-performance materials are essential. Monel 400 sheets, plates, and coils are widely sought after by importers, suppliers, stockists, and exporters due to their unique properties and extensive usability across industries like marine, chemical processing, oil and gas, and aerospace.
Monel 400 exhibits exceptional resistance to corrosion in acidic and alkaline environments. Its high tolerance to saltwater, brine, and chloride-containing conditions makes it a preferred material for marine engineering and desalination plants.
These sheets, plates, and coils also showcase remarkable thermal conductivity and mechanical strength, enabling them to perform well under high-temperature conditions. Additionally, Monel 400’s ability to withstand stress corrosion cracking and pitting ensures longevity and reliability, even in challenging operating conditions.
Monel 400 sheets, plates, and coils are extensively used in industries requiring durable and corrosion-resistant materials. In marine engineering, these products are essential for constructing ship components, propeller shafts, and pump components due to their ability to resist seawater corrosion. In the chemical and petrochemical industries, Monel 400 is used for manufacturing heat exchangers, pressure vessels, and storage tanks. Its strength and resistance to oxidation also make it a preferred choice for aerospace components and power generation equipment.
Monel 400’s unmatched corrosion resistance, durability, and adaptability make it a preferred choice for demanding applications. Its versatility ensures that importers, suppliers, stockists, and exporters can cater to a wide range of industries. Whether it’s for constructing offshore platforms, handling chemical processes, or building aerospace components, Monel 400 remains an indispensable material for projects requiring longevity and reliability. By choosing Monel 400 sheets, plates, and coils from trusted global suppliers, industries can secure the materials they need to achieve operational excellence and long-term success.
| UNS No. | N04400 |
|---|---|
| Standard | Monel 400 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Monel 400 | 2.4360 | N04400 | 63.00 Min | - | - | - | 2.5 Max | 28.0 - 34.0 | - | - | - | 0.30 Max | 0.024 Max | 0.50 Max | 2.0 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Monel 400 | 550 | 275 | 30 | 8.80 |