Monel K500 Pipe is made up of a work hardenable nickel copper alloy. The material has high strength, corrosion resistance and it is non – magnetic. These are used in cable wraps, marine equipment, submarine parts, valve trays and in electronic components. Delta Superalloys is a leading supplier of these Monel K500 Pipe products in various sizes and types.
The pipes come under the ASTM B163 and ASTM B165 specifications. These specifications abide by the ASTM, ASME and API standards. The sizes of the Monel K500 Tube range from 15NB to 150NB with the thicknesses ranging from 0.6mm to 20mm. The outer diameter of the tubes range from 6.35mm to 254mm. The UNS N05500 Tubing can come in different lengths such as single random, double random or cut to length sizes.
The ends of the pipes can vary. The pipes can be plain ended, beveled ended or treaded. There are seamless, ERW, welded and fabricated pipes.The K500 Monel Seamless Pipe has less absolute roughness and is dimensionally more accurate than the other forms of pipes. The pipes can also be round or hydraulic in form. The chemical composition of the material has 63% nickel, 27% copper and titanium, iron, silicon, manganese, aluminum and carbon.
This composition provides the ASME SB165 Monel Welded Pipe with 790MPa minimum yield strength and 1100MPa minimum tensile strength. The melting point of the pipes is also high at 1350 degrees Celsius. This means that the pipes can operate under high temperatures. Please feel free to contact us for more information on the different products such as the K500 Monel Alloy ERW Pipe and the prices.
Monel K500 is an extremely versatile nickel-copper alloy that offers superior corrosion resistance properties in freshwater and saltwater environments and exceptional strength at elevated temperatures when compared with other alloys. Its machinability also allows Monel K500 ERW Tubes to be easily formed into complex shapes without sacrificing their structural integrity, making it ideal for various uses, from heat exchangers to aerospace components such as turbine blades and exhaust systems.
| UNS No. | N05500 |
|---|---|
| Standard | Monel K500 Pipes & Tubes |
| Pipe Size | 1/8" NB to 36" NB |
| Schedule | SCH5, SCH10, SCH10S, SCH40, SCH40S, SCH80, SCH80S, SCH160, SCH160S, SCHXXS |
| Type | Seamless, Welded, EFW, Fabricated |
| Tube Size | 4mm od to 50mm od |
| Thickness | 0.3mm to 5mm thk |
| Length | 100mm to 6000mm, Custom Cut length |
| End | Plain End, Threaded end |
| Form | Round, Square, Triangle etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Monel K-500 | 2.4375 | N05500 | 63.00 Min | - | - | - | 2.0 Max | 27.0 - 33.0 | - | 2.30 - 3.15 | 0.35 - 0.85 | 0.25 Max | 0.01 Max | 0.50 Max | 1.5 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Monel K-500 | 1000 | 655 | 40 | 8.44 |