Monel K500 Sheets, Plates & Coils are versatile materials that are widely used in various industries due to their outstanding strength, corrosion resistance, and durability. This alloy, primarily made of nickel (63%), copper (27%), and small amounts of aluminum (2.3%) and titanium (0.35%), combines the excellent properties of Monel with the added strength and hardness imparted by the titanium.
Monel K500 is especially known for its high resistance to sea water, acids, alkalis, and other corrosive environments, making it an ideal choice for marine, chemical, and aerospace applications.Monel K500 Sheets are widely used in industries requiring materials that can withstand extreme conditions, including saltwater exposure and high temperatures.
The alloy's exceptional mechanical properties—such as its high tensile strength, excellent fatigue and thermal-fatigue strength, and superior resistance to cavitation and erosion—make it an ideal material for manufacturing components that demand high performance. The Monel K500 Plates offer versatility in design and fabrication, allowing for easy machining and welding. These plates are commonly used in the production of valves, pumps, and marine propellers.
Monel K500 Coils are another form of the alloy that provides enhanced flexibility, making them suitable for industries that require materials to be formed into various shapes and sizes. The coils are particularly beneficial for industries in need of large quantities of the material for continuous operations. This type of Monel alloy offers great resistance to oxidation and corrosion, even in high temperatures, and is used in applications such as aerospace, electronics, and chemical processing.
Monel K500 is highly favored by importers, suppliers, stockists, and exporters around the world due to its superior quality and durability. As importers, they ensure that the alloy meets international standards and is sourced from reputable manufacturers. Suppliers provide Monel K500 Sheets, Plates, and Coils in various sizes and thicknesses to meet the specific requirements of their customers. Stockists play a crucial role in maintaining inventory and ensuring the timely availability of Monel K500 products for various industries. Additionally, Monel K500 is exported globally, where it is used in high-performance applications across different sectors, including oil and gas, shipbuilding, power generation, and more.
| UNS No. | N10276 |
|---|---|
| Standard | Monel K500 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Monel K-500 | 2.4375 | N05500 | 63.00 Min | - | - | - | 2.0 Max | 27.0 - 33.0 | - | 2.30 - 3.15 | 0.35 - 0.85 | 0.25 Max | 0.01 Max | 0.50 Max | 1.5 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Monel K-500 | 1000 | 655 | 40 | 8.44 |