Nickel 200 forged products are known for their excellent corrosion resistance, high strength, and versatility, making them ideal for a variety of industrial applications. Nickel 200, a pure nickel alloy, consists of 99.6% nickel, and it is widely used across industries that require materials resistant to corrosion, especially in harsh environments. As a result, it has become a go-to choice for sectors like chemical processing, food production, aerospace, and electronics.
One of the key attributes of Nickel 200 forged products is their ability to withstand a wide range of temperatures and aggressive chemicals. They exhibit remarkable resistance to alkaline and neutral salt solutions, making them suitable for use in marine environments. These products also offer outstanding thermal and electrical conductivity, which further enhances their demand in industries such as electronics, where efficient heat dissipation and conductivity are crucial. Additionally, the material has a low rate of thermal expansion, allowing it to maintain structural integrity even under extreme temperature changes.
Nickel 200 forged products come in various forms such as bars, rods, plates, sheets, pipes, and fittings. These products are often used in the construction of pressure vessels, heat exchangers, reactors, and other high-performance equipment. The forging process used to create these products ensures enhanced mechanical properties, such as improved toughness and strength. It also allows for the creation of complex shapes and customized dimensions, catering to the specific needs of diverse industries.
Exporters also play a crucial role in delivering Nickel 200 forged products to global markets. With increasing demand for this material worldwide, experienced exporters ensure timely delivery while maintaining the quality of the products. Their expertise in logistics and trade regulations helps facilitate smooth transactions, making it easier for businesses across the globe to access top-quality Nickel 200 forged products.
Nickel 200 forged products are a valuable choice for industries requiring high-performance, corrosion-resistant materials. Whether sourcing from reliable importers, suppliers, stockists, or exporters, businesses can count on the versatility and durability of Nickel 200 for a wide range of applications.
| UNS No | N02200 |
|---|---|
| Standard | Nickel 200 Forged Products |
| Circle | 5mm dia to 2000mm dia |
| Thickness | 6mm thk to 500mm thk |
| Flat Bar Blocks | 5mm thk to 500mm thk |
| Rings | 50mm dia to 1000mm dia |
| Rounds, shafts | 6mm dia to 500mm dia |
| Hex Bar | 6mm dia to 500mm dia |
| Cylinder and sleeves | 6mm dia to 500mm dia |
| Finish | Black or Bright |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Nickel 200 | 2.4066 2.4060 | N02200 | 99.00 Min | - | - | - | 0.40 Max | 0.25 Max | - | - | - | 0.15 Max | 0.010 Max | 0.35 Max | 0.35 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Nickel 200 | 415 | 105 | 35 | 8.89 |