Nickel 200 sheets, plates, and coils are highly sought after in a wide range of industries due to their exceptional properties and versatility. Manufactured from commercially pure wrought nickel (99.6% minimum), Nickel 200 is renowned for its excellent corrosion resistance, high thermal and electrical conductivity, and outstanding mechanical properties. These characteristics make it a preferred choice for applications in chemical processing, marine engineering, aerospace, and energy industries.
As a leading material for various demanding environments, Nickel 200 sheets are extensively used in fabricating components that require strong resistance to acids, alkalis, and other corrosive agents. They are particularly effective in handling caustic soda, sulfuric acid, and hydrochloric acid environments. The superior ductility of these sheets ensures easy machinability and forming, making them ideal for producing high-performance equipment. Similarly, Nickel 200 plates offer robustness and durability, making them suitable for heavy-duty applications such as heat exchangers, pressure vessels, and storage tanks.
Nickel 200 coils are highly versatile and can be tailored for custom applications. Their excellent weldability and seamless surface finish ensure they meet stringent industry standards. These coils are widely used in industries where precise dimensional tolerances and high-quality material are critical, such as electronics, automotive, and power generation. Moreover, their non-magnetic properties and excellent resistance to extreme temperatures enhance their usability in specialized applications.
Nickel 200 products are not only durable but also sustainable, as they can be recycled without losing their inherent properties. This makes them an eco-friendly choice for industries striving to reduce environmental impact. As demand for high-performance materials continues to grow, the importance of connecting with trusted Nickel 200 suppliers and exporters cannot be overstated.
Nickel 200 sheets, plates, and coils are indispensable in various industries due to their superior chemical resistance, mechanical strength, and adaptability. Whether you are seeking to source these materials locally or internationally, partnering with reliable importers, suppliers, stockists, and exporters ensures you receive high-quality products tailored to your requirements. From manufacturing durable components to meeting precise industry standards, Nickel 200 remains a trusted choice for applications where reliability and performance are paramount.
| UNS No. | N02200 |
|---|---|
| Standard | Nickel 200 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Nickel 200 | 2.4066 2.4060 | N02200 | 99.00 Min | - | - | - | 0.40 Max | 0.25 Max | - | - | - | 0.15 Max | 0.010 Max | 0.35 Max | 0.35 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Nickel 200 | 415 | 105 | 35 | 8.89 |