Nickel 200 is a highly versatile and pure nickel alloy that offers exceptional resistance to a wide range of corrosive environments. Known for its outstanding mechanical properties and thermal conductivity, Nickel 200 is widely used in industrial applications where durability and resistance to oxidation are critical. Among the various forms of this alloy, Nickel 200 wires, flanges, and fasteners are particularly valued for their functionality, reliability, and adaptability.
Nickel 200 wires are extensively used in electrical and electronic applications due to their excellent conductivity and corrosion resistance. These wires are highly sought after in industries such as aerospace, marine, chemical processing, and electronics manufacturing. With superior malleability and ductility, Nickel 200 wires are suitable for complex designs and demanding environments. L
Leading suppliers, importers, and stockists ensure that these wires are available in various diameters and lengths to meet the diverse needs of customers globally. Exporters of Nickel 200 wires cater to international markets by adhering to stringent quality standards and providing timely deliveries.
Nickel 200 fasteners, including bolts, nuts, screws, and washers, are designed to deliver exceptional performance in corrosive and high-temperature environments. These fasteners are extensively used in applications where reliability and strength are non-negotiable, such as in marine engineering, chemical processing plants, and heat exchangers. Importers and suppliers ensure the availability of a wide range of fasteners in standard and customized specifications. Exporters play a crucial role in meeting the requirements of global industries, ensuring that fasteners conform to international standards like ASTM and ASME.
Importers, suppliers, stockists, and exporters of Nickel 200 wires, flanges, and fasteners play an integral role in ensuring seamless supply chains for industries worldwide. Stockists maintain a ready inventory of these products to cater to immediate requirements, while suppliers provide comprehensive solutions tailored to specific needs. Importers focus on sourcing high-quality materials from reliable manufacturers, and exporters ensure that these products reach international clients efficiently.
| UNS No | N02200 |
|---|---|
| Standard | Nickel 200 Wires |
| Diameter | 0.1mm to 100mm |
| Length | 100mm to 6000mm, Custom Cut Length |
| Form | Filler Wire, Coil Wire, Wire, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Nickel 200 | 2.4066 2.4060 | N02200 | 99.00 Min | - | - | - | 0.40 Max | 0.25 Max | - | - | - | 0.15 Max | 0.010 Max | 0.35 Max | 0.35 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Nickel 200 | 415 | 105 | 35 | 8.89 |