We are providing Hastelloy C22 forged products in several sizes, types, shapes, grades and standards. We are supplying these forged products in custom made specifications as per the demands. Hastelloy C22 has exceptional resistance to crevice corrosion and pitting. This alloy contains chromium, iron, molybdenum and tungsten. These elements provide excellent corrosion resistance in acidic and chloride environments.
We have a highly experienced manufacturing team who ensures to use the superior quality raw material to develop Hastelloy C22 Forged products. Our company collects this material from trustworthy market vendors. Our team accomplishes the development of the product by following the guidelines of national and international quality standards. We carry out the assembly of Hastelloy C22 Forged products under the strict inspection of our experts.
Our well-trained workers and professionals use modern tools and refined technology to manufacture these forged products. These fittings offer excellent resistance to intergranular corrosion and stress corrosion cracking.Delta Superalloys is exporting a premium range of Hastelloy C22 Forged products to domestic as well as global industries.
These forged products are suitable for many applications such as Gas processing, Oil refineries, chemical industries, pressure vessels, pharmaceutical, boilers, paper and pulp industries, heat exchangers, petrochemical industries and condensers. We carry out the development of products in our highly equipped manufacturing unit. We are producing Hastelloy C22 Forged products having various quality features such as high mechanical strength, perfect dimensional accuracy, excellent anti-corrosiveness, high durability, superior surface finish and long working life.
| UNS No | N06022 |
|---|---|
| Standard | Hastelloy C22 Forged Products |
| Circle | 5mm dia to 2000mm dia |
| Thickness | 6mm thk to 500mm thk |
| Flat Bar Blocks | 5mm thk to 500mm thk |
| Rings | 50mm dia to 1000mm dia |
| Rounds, shafts | 6mm dia to 500mm dia |
| Hex Bar | 6mm dia to 500mm dia |
| Cylinder and sleeves | 6mm dia to 500mm dia |
| Finish | Black or Bright |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C22 | 2.4602 | N06022 | Remainder | 20.0 - 22.5 | 2.5 Min | 12.5 - 14.5 | 2.0 - 6.0 | - | - | - | - | 0.015 Max | 0.02 Max | 0.08 Max | 0.50 Max | W - 2.5-3.5 / V - 0.35 Min / P - 0.02 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy C22 | 690 | 310 | 45 | 8.69 |