Hastelloy is an austenitic super alloy, which is highly versatile. The Hastelloy C22 Round Bar is made with a chemical concentration of 22% chromium, 14% molybdenum, and 3% tungsten. These tubes are highly resistant to all forms of corrosion. The Hastelloy C22 ASTM B574 Flat Bar is designed with good mechanical properties. They possess a tensile strength of a minimum 690Mpa and yield strength of a minimum 310Mpa.
The Hastelloy B574 Hollow Bar is used in applications, which requires it to function in extreme pressure and high temperatures. These bars can be easily elongated by 45% and still possess excellent workability. The ASTM B574 Hastelloy C22 Rod provides protection against various acids and oxidation agents along with several reducing media. They possess a density of about 8.69 g/cm3.
Hastelloy Alloy C22 Round Rod is used to provide support to existing structures. These rods have excellent strength and superior electrical conductivity. They can suffice in temperatures up to 1250 degrees F. The Hastelloy C22 Bar is widely used in chemical industries, paper, and pulp production, pollution control, marine applications, waste treatment systems, etc. We are the leading supplier and manufacturer of the Alloy C22 Round Bar. Our mission is to produce and supply high-quality products, which are available at reasonable rates.
Being prominent suppliers and stockists, Delta Superalloys maintains a comprehensive inventory of Hastelloy C22 round bars in various sizes, dimensions, and finishes. This ensures timely delivery of materials, even for urgent requirements. The company’s extensive distribution network allows it to serve clients across multiple regions seamlessly. Moreover, Delta Superalloys offers customized solutions, catering to the specific needs of industries ranging from oil and gas to pharmaceuticals.
The ASTM B574 Alloy N06022 Hex Bar acts as a connector between the center and the bar. They are widely used in pressure valves as a plug to stop excess pressure. These bars are manufactured following all ASTM standards. In the Hastelloy C22 N06022 Hexagon Bars, sizes are available between 6mm to 105mm. They are precisely made for systems and machines, which require pieces of accurate sizes.
| UNS No | N06022 |
|---|---|
| Standard | Hastelloy C22 Round Bars |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm thickness |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Thickness | 1.6mm to 100mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Round Bar, Square Bar, Hex(A/F) Bar, Rectangle Bar, Billet, Ingot, Forging, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C22 | 2.4602 | N06022 | Remainder | 20.0 - 22.5 | 2.5 Min | 12.5 - 14.5 | 2.0 - 6.0 | - | - | - | - | 0.015 Max | 0.02 Max | 0.08 Max | 0.50 Max | W - 2.5-3.5 / V - 0.35 Min / P - 0.02 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy C22 | 690 | 310 | 45 | 8.69 |