We as a importers, suppliers, stockists, and exporters offer a wide range Hastelloy C22 Sheets in Delta Superalloys. Hastelloy C22 Plates (UNS N06022) are used in Scrubbers, Heat exchangers, Reaction vessels, Evaporators and more. Welding can be done by gas tungsten-arc, gas metal-arc and shielded metal-arc processes. Our Alloy C22 Sheets can be cut using any conventional plasma arc cutting system. The best arc quality is achieved using a mixture of argon and hydrogen gases.
Hastelloy C22 sheets and Hastelloy C22 plates are among the most preferred materials for solving corrosion-related problems. Hastelloy C22 is a high-temperature alloy with good mechanical properties. It is suitable for heat exchangers, oil and gas processing equipment components, pollution control systems, and nuclear fuel reprocessing components. Its superior resistance to stress corrosion cracking will prevent cracks in areas subjected to dynamic stresses..
Hastelloy C276 and Hastelloy C22 plates are both widely used in the metalworking industry. Hastelloy C276 is known for its corrosion resistance, tensile strength and formability, while Hastelloy C22 sheets and plates are valued for their superior durability and weldability. Hastelloy C276 has a higher chromium content than Hastelloy C22, which gives it excellent pitting and crevice corrosion resistance.
Hastelloy C22 has a chemical composition that makes it superior to Hastelloy C276 in terms of chlorine stress corrosion cracking resistance. Both Hastelloy alloys are resistant to many acids and various types of chemicals, but overall, Hastelloy C22 has slightly greater versatility than Hastelloy C276.
| UNS No. | N06022 |
|---|---|
| Standard | Hastelloy C22 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C22 | 2.4602 | N06022 | Remainder | 20.0 - 22.5 | 2.5 Min | 12.5 - 14.5 | 2.0 - 6.0 | - | - | - | - | 0.015 Max | 0.02 Max | 0.08 Max | 0.50 Max | W - 2.5-3.5 / V - 0.35 Min / P - 0.02 Max |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy C22 | 690 | 310 | 45 | 8.69 |